Home / Custom siliconization
Custom siliconization of glass and polymer syringes
Glass and polymer syringes re-siliconized to the silicone levels your study needs, verified by weight and by distribution scan, in lots from a few samples up to 5,000.
Why silicone level matters
Silicone oil is the lubricant that lets a plunger stopper move in a syringe barrel. How much there is, and how evenly it covers the barrel, affects most of what the system does.
Too little silicone, or a patchy layer, raises break-loose and glide force and can lengthen injection time in an autoinjector. Too much puts more droplets into solution, where they count as sub-visible particles. Silicone also moves over time, so a syringe that glides well at time zero can stick at twelve months.
A supplier's specification allows a range, and the syringes you receive for development usually sit somewhere inside it, not at the edges. Custom siliconization lets you test the edges deliberately, which is the only way to know your product and device have margin across what the supplier is allowed to ship.
What we do
We start from your as-received glass or polymer syringe barrels and return study-ready syringes at the silicone levels you specify.
Preparation
A known starting point, a known target and a measured result.
As-received mapping
Silicone coverage is mapped over the full inner surface of the as-received barrels. The scan is non-destructive, so the baseline is taken on the units that go on through the process.
Strip and clean
Barrels are stripped of their existing silicone and cleaned, so that every unit starts from the same condition.
Re-siliconization to target
Silicone is applied to the target levels you define, including the low and high ends of a supplier's specification. We spray silicone oil (Dow Corning 360, 1,000 to 12,500 cSt) with fixed or diving nozzles, or apply a silicone emulsion (Dow Corning 365 or 366) that is then baked on. Spray loads run from about 0.25 mg for low-silicone biologics syringes up to standard loads of 0.6 to 0.8 mg.
Verification
Each target level is confirmed by silicone weight and by distribution scan before the containers leave the lab.
Study-ready containers
What happens after the silicone is on.
Packaging and sterilization
Re-siliconized barrels are packaged. Dry-heat (oven) sterilization is done in house by Kiln. If the syringes need to be autoclaved, or sterilized by ethylene oxide (EtO) or gamma irradiation, that work is done by a qualified partner.
Filling and assembly
Syringes can be filled at Kiln with placebo, WFI or a surrogate solution, and assembled into your device. See filling and assembly and packaging.
Functional testing
Break-loose and glide force, and injection time in your device, measured on the low, nominal and high lots at time zero and across aging.
Particles
Sub-visible particle imaging on the same lots shows how silicone level changes what moves into solution.
How we work
Work is structured in phases with clear deliverables at each gate, so you always know what you have paid for and what comes next.
-
Scope
We agree the container, the target silicone levels, the quantities and what testing follows.
-
Map
As-received barrels are scanned for silicone distribution to set the baseline.
-
Prepare
Barrels are stripped, cleaned and re-siliconized to each target level.
-
Verify
Each target level is confirmed by silicone weight and by distribution scan.
-
Deliver
Syringes are packaged and sterilized (dry heat in house, or autoclave, EtO or gamma through a qualified partner), then ship to you or move into filling and testing at Kiln.
Deliverables
Deliverables are defined in the proposal before work starts. A typical engagement includes the following.
Related services
Questions we hear often
If yours isn't here, it's a good thing to bring to a consultation.
Why test at the low and high ends of the silicone specification?
Because syringes at the edges of the specification can behave differently from the ones you received for development. Low silicone can raise glide force and lengthen injection time. High silicone can increase silicone droplets in solution. Testing at both ends shows whether your product and device have margin across the range a supplier is allowed to ship.
How do you verify the silicone level?
By silicone weight and by a distribution scan of the barrel. The scan is non-destructive, so the same unit can be followed through filling and aging.
Which formats and lot sizes do you handle?
Glass and polymer syringes, in lots from a few samples up to 5,000.
Do the syringes come back ready to fill?
Yes. We package the re-siliconized barrels and sterilize them. Dry-heat (oven) sterilization is done in house. Autoclave, ethylene oxide (EtO) or gamma sterilization is done by a qualified partner.
Can you run the testing on the custom syringes as well?
Yes. Filling, break-loose and glide force, device testing and sub-visible particle imaging can all be run at Kiln on the same lots.
Need syringes at a specific silicone level?
Tell us the container, the silicone targets and what you plan to test. We'll set up a call to talk through quantities and timing.
Prefer email? Write to info@kiln-lab.com or call +1 (866) 350-8240.